镁合金钢板内固定治疗胫骨中段骨折的有限元分析
PDF下载 (253)徐景超,张雁儒,杨 越,李 昊,李洁洁,余进伟.镁合金钢板内固定治疗胫骨中段骨折的有限元分析[J].宁波大学学报(理工版),2022,35(4):109-114.DOI:
XU Jingchao,ZHANG Yanru,YANG Yue,LI Hao,LI Jiejie,YU Jinwei.Finite element analysis research of magnesium alloy plate internal fixation for middle tibial fracture[J].Journal of Ningbo University(Natural Science & Engineering Edition),2022,35(4):109-114.DOI:
| Title: | Finite element analysis research of magnesium alloy plate internal fixation for middle tibial fracture |
| 作者: | 徐景超, 张雁儒, 杨 越, 李 昊, 李洁洁, 余进伟 |
| Author(s): | XU Jingchao, ZHANG Yanru, YANG Yue, LI Hao, LI Jiejie, YU Jinwei |
| 关键词: | 胫骨中段骨折; 镁合金; 钛合金; 不锈钢; 有限元分析; 内固定 |
| Keywords: | middle tibial fracture; magnesium alloy; titanium alloy; stainless steel; finite element analysis; internal fixation |
| 分类号: | R608 |
| 文献标识码: | A |
| 摘要: | 运用有限元分析法, 评价镁合金、钛合金、不锈钢3种不同材料在治疗胫骨干骨折的力学性能差异. 以Dicom格式导入Mimics 20.0软件中建立胫骨三维模型, 并运用Geomagic与Solidwork软件制作胫骨骨折内固定模型, 将上述模型导入Workbench 2020软件中, 赋予材料属性, 给予轴向载荷、扭转载荷2种加载模式, 分析3种材料的应力和位移. 在600N轴向加载模式下, 钛合金内固定应力为(117.42±0.07)MPa, 位移为(0.73±0.11)mm; 镁合金内固定应力为(117.11±0.04)MPa, 位移为(0.82±0.08)mm; 不锈钢内固定应力为(117.53±0.03)MPa, 位移为(0.62±0.13)mm. 在30N?mm扭转加载模式下, 钛合金内固定应力为(174.50±0.33)MPa, 位移为(0.75±0.07)mm; 镁合金内固定应力为(168.75±0.15)MPa, 位移为(0.82±0.16)mm; 不锈钢内固定应力为(176.23±0.51)MPa, 位移为(0.61±0.13)mm. 结果表明: 2种不同加载模式下3种不同材料的内固定结果数值差异不大, 镁合金内固定与钛合金内固定、不锈钢内固定力学性能相似, 而镁合金更亲和人体, 可以代替传统医用金属材料用以治疗胫骨中段骨折. |
| Abstract: | The present study was designed to evaluate the mechanical properties of magnesium alloy, titanium alloy and stainless steel in the treatment of tibial shaft fracture by using finite element analysis method. A case of high-definition tibia CT data was selected and imported into Mimics 20.0 software in Dicom format. A three-dimensional model of tibia was established. Both Geomagic and Solidwork software packages were used to make internal fixation model of tibia fracture. The model was then imported into Workbench 2020 software with the material attributes specified. Two loading modes, the axial and torsional loading, were given to analyze the stress and displacement of the two materials. Under 600 N axial loading mode, the internal fixed stress of titanium alloy was (117.42±0.07) MPa and the displacement was (0.73±0.11) mm. The internal fixed stress of magnesium alloy was (117.11±0.04) MPa and the displacement was (0.82±0.08) mm. The internal fixed stress of stainless steel was (117.53±0.03) MPa and the displacement was (0.62±0.13) mm. The internal fixed stress of titanium alloy was (174.50±0.33) MPa and the displacement was (0.75±0.07) mm under the torsional loading mode of 30 N?mm. The internal fixed stress of magnesium alloy was (168.75±0.15) MPa and the displacement was (0.82±0.16) mm. The internal fixed stress of stainless steel was (176.23±0.51) MPa and the displacement was (0.61±0.13) mm. The results of internal fixation of three groups of different materials under two different loading modes were not significantly different. The results show that the mechanical properties of magnesium alloy internal fixation are similar to those of traditional titanium alloy internal fixation and stainless steel internal fixation. Moreover, magnesium alloy is better for the human body and may replace the traditional medical metal materials in the treatment of mid-segment tibial fracture. |
| 参考文献 /References: | [1] Lan C B, Wu Y, Guo L L, et al. Effects of cold rolling on microstructure, texture evolution and mechanical properties of Ti-32.5Nb-6.8Zr-2.7Sn-0.3O alloy for biomedical applications[J]. Materials Science and Engineering: A, 2017, 690:170-176. [2] Owaid M N, Ibraheem I J. Mycosynthesis of nanoparticles using edible and medicinal mushrooms[J]. European Journal of Nanomedicine, 2017, 9(1):5-23. [3] Limmahakhun S, Oloyede A, Sitthiseripratip K, et al. Stiffness and strength tailoring of cobalt chromium graded cellular structures for stress-shielding reduction[J]. Materials & Design, 2017, 114:633-641. [4] Taheri A M, Saedi S, Turabi A S, et al. Mechanical and shape memory properties of porous Ni50.1Ti49.9 alloys manufactured by selective laser melting[J]. Journal of the Mechanical Behavior of Biomedical Materials, 2017, 68:224-231. [5] 袁广银, 牛佳林. 可降解医用镁合金在骨修复应用中的研究进展[J]. 金属学报, 2017, 53(10):1168-1180. [6] Li G Y, Zhang L, Wang L, et al. Dual modulation of bone formation and resorption with zoledronic acid-loaded biodegradable magnesium alloy implants improves osteoporotic fracture healing: An in vitro and in vivo study[J]. Acta Biomaterialia, 2018, 65:486-500. [7] Berglund I S, Dirr E W, Ramaswamy V, et al. The effect of Mg-Ca-Sr alloy degradation products on human mesenchymal stem cells[J]. Journal of Biomedical Materials Research Part B: Applied Biomaterials, 2018, 106(2):697-704. [8] 刘国光. 不同固定方法治疗167例胫骨骨折的病例对照研究[J]. 中外医学研究, 2017, 15(6):115-116. [9] Ai J, Kan S L, Li H L, et al. Anterior inferior plating versus superior plating for clavicle fracture: A meta-analysis[J]. BMC Musculoskeletal Disorders, 2017, 18(1):159. [10] 周凯华, 陶星光, 梁会, 等. 基于有限元分析比较碳纤维增强聚醚醚酮复合板与钛制钢板固定胫骨中段骨折的效果[J]. 中国骨与关节损伤杂志 2020, 35(10):1028-1032. [11] Mitkovic M, Milenkovic S, Micic I, et al. Results of the femur fractures treated with the new selfdynamisable internal fixator (SIF)[J]. European Journal of Trauma and Emergency Surgery: Official Publication of the European Trauma Society, 2012, 38(2):191-200. [12] Bottlang M, Lesser M, Koerber J, et al. Far cortical locking can improve healing of fractures stabilized with locking plates[J]. The Journal of Bone and Joint Surgery American Volume, 2010, 92(7):1652-1660. [13] 袁广银, 章晓波, 牛佳林, 等. 新型可降解生物医用镁合金JDBM的研究进展[J]. 中国有色金属学报, 2011, 21(10):2476-2488. [14] 郑玉峰, 顾雪楠, 李楠, 等. 生物可降解镁合金的发展现状与展望[J]. 中国材料进展, 2011, 30(4):30-43; 29. [15] Dziuba D, Meyer-Lindenberg A, Seitz J M, et al. Long-term in vivo degradation behaviour and biocompatibility of the magnesium alloy ZEK100 for use as a bio-degradable bone implant[J]. Acta Biomaterialia, 2013, 9(10):8548-8560. [16] Wu Y F, Wang Y M, Zhao D W, et al. In vivo study of microarc oxidation coated Mg alloy as a substitute for bone defect repairing: Degradation behavior, mechanical properties, and bone response[J]. Colloids and Surfaces B: Biointerfaces, 2019, 181:349-359. [17] Wong C C, Wong P C, Tsai P H, et al. Biocompatibility and osteogenic capacity of Mg-Zn-Ca bulk metallic glass for rabbit tendon-bone interference fixation[J]. International Journal of Molecular Sciences, 2019, 20(9):2191. [18] Weng W J, Biesiekierski A, Li Y C, et al. A review of the physiological impact of rare earth elements and their uses in biomedical Mg alloys[J]. Acta Biomaterialia, 2021, 130:80-97. [19] Willbold E, Gu X N, Albert D, et al. Effect of the addition of low rare earth elements (lanthanum, neodymium, cerium) on the biodegradation and biocompatibility of magnesium[J]. Acta Biomaterialia, 2015, 11:554-562. [20] 张余, 马立敏, 蓝国波, 等. 镁合金与钛合金经口咽前路寰枢椎复位内固定钢板治疗寰枢椎脱位的三维有限元分析[J]. 中华创伤杂志, 2012, 28(10):921-925. |