镁合金空心螺钉内固定治疗股骨颈骨折的有限元分析研究
PDF下载 (250)方永刚,徐景超,张雁儒,杨 越,李 昊,李洁洁.镁合金空心螺钉内固定治疗股骨颈骨折的有限元分析研究[J].宁波大学学报(理工版),2022,35(1):7-10.DOI:
FANG Yonggang,XU Jingchao,ZHANG Yanru,YANG Yue,LI Hao,LI Jiejie.Finite element analysis research of magnesium alloy cannulated screw internal fixation for femoral neck fracture[J].Journal of Ningbo University(Natural Science & Engineering Edition),2022,35(1):7-10.DOI:
| Title: | Finite element analysis research of magnesium alloy cannulated screw internal fixation for femoral neck fracture |
| 作者: | 方永刚, 徐景超, 张雁儒, 杨 越, 李 昊, 李洁洁 |
| Author(s): | FANG Yonggang, XU Jingchao, ZHANG Yanru, YANG Yue, LI Hao, LI Jiejie |
| 关键词: | 股骨颈骨折; 镁合金; 钛合金; 有限元分析 |
| Keywords: | femoral neck fracture; magnesium alloy; titanium alloy; finite element analysis |
| 分类号: | R615 |
| 文献标识码: | A |
| 摘要: | 利用有限元分析方法探究镁合金空心螺钉内固定治疗股骨颈骨折的生物力学特性, 旨在为临床治疗股骨颈骨折提供一种新的思路. 选取一例青年健康志愿者的下肢CT数据建立股骨三维模型, 在Mimics插件3-matic中建立股骨网格并赋予网格材料属性, 利用Solidworks 17.0软件建立空心螺钉模型, 将上述2个三维模型导入Workbench 2020软件中, 分别赋予空心螺钉镁合金、钛合金材料属性, 进行对比分析, 记录股骨及空心螺钉的峰值、应力分布值和股骨位移. 结果表明, 钛合金螺钉内固定模型最大应力为357.27MPa, 最大位移为0.034mm; 镁合金螺钉内固定模型最大应力为311.27MPa, 最大位移为0.034mm; 2组不同材料的空心钉结果数值差异不大. 研究表明镁合金空心螺钉和传统钛合金空心螺钉力学性能相似, 且镁合金更加亲和人体, 在临床方面可以镁合金空心螺钉代替钛合金空心螺钉治疗股骨颈骨折. |
| Abstract: | This research explores the biomechanical properties of magnesium alloy hollow screw internal fixation for the treatment of femoral neck fractures by finite element analysis, with an intention to provide new ideas for the clinical treatment of femoral neck fractures. A case of young healthy volunteers’ lower limb CT data was stored and a three-dimensional femoral model was established. The femoral mesh was established in the Mimics plug-in module “3-matic”, with which the mesh material properties were assigned. Subsequently, Solidworks 17.0 software was used to establish a hollow screw model. The above two 3D models were then input into Workbench 2020 software, where they were assigned with the hollow screw magnesium alloy and titanium alloy material properties for comparative analysis. The peak value, stress distribution value and femoral displacement of the femur and the hollow screw from the analysis were recorded. The maximum stress of the titanium alloy screw internal fixation model was 357.27MPa, and the maximum displacement was 0.034mm. On the contrary, the maximum stress of the internal fixation model of magnesium alloy screws was 311.27MPa, and the maximum displacement was 0.034mm. Hence, there is little difference in the results of hollow nails of different materials between the two groups. It can be concluded that the mechanical properties of magnesium alloy hollow screws are similar to those of the traditional titanium alloy hollow screws, and magnesium alloys are more compatible with the human body. Therefore, it is possible to consider using magnesium alloy hollow screws instead of titanium alloy hollow screws to treat femoral neck fractures. |
| 参考文献 /References: | [1] Torkian A, Faraji G, Pedram M S. Mechanical properties and in vivo biodegradability of Mg-Zr-Y-Nd-La magnesium alloy produced by a combined severe plastic deformation[J]. Rare Metals, 2021, 40(3):651-662. [2] 孙兴文, 董黎敏, 李炫, 等. 镁合金与钛合金接骨板在股骨骨折愈合中力学性能的研究[J]. 天津理工大学学报, 2017, 33(3):49-54. [3] Amano H, Hanada K, Hinoki A, et al. Biodegradable surgical staple composed of magnesium alloy[J]. Scientific Reports, 2019, 9:14671. [4] 尚晓峰, 窦坚, 韩青. 基于Abaqus下植入体与股骨腔配合的有限元分析[J]. 临床骨科杂志, 2018, 21(3):373-375. [5] Freitas A, Bontempo R L, Azevedo F, et al. New fixation method for Pauwels type III femoral neck fracture: A finite element analysis of sliding hip screw, L-shaped, and L-shaped with medial plate[J]. European Journal of Orthopaedic Surgery & Traumatology: Orthopedie Traumatologie, 2021, 31(6):1069-1075. [6] Ramadanov N, Toma I, Herkner H, et al. Factors that influence the complications and outcomes of femoral neck fractures treated by cannulated screw fixation[J]. Scientific Reports, 2020, 10:758. [7] Rao M J, Zhang G H, Yuan X J, et al. Internal fixation versus total hip arthroplasty in the treatment of displaced femoral neck fracture: A meta-analysis of randomized controlled trials[J]. Biomedical Journal of Scientific & Technical Research, 2021, 33(5):26233-26238. [8] Xu W N, Xue Q Y. Long-term efficacy of screw fixation vs hemiarthroplasty for undisplaced femoral neck fracture in patients over 65 years of age: A systematic review and metal-analysis[J]. Orthopaedic Surgery, 2021, 13(1):3-13. [9] 殷浩, 周恩昌, 潘政军, 等. 4枚空心钉与3枚空心钉结合支持钢板内固定治疗Pauwels Ⅲ型股骨颈骨折的有限元分析[J]. 中国组织工程研究, 2019, 23(32):5133-5137. [10] Chandra G, Pandey A. Design and analysis of biodegradable buttress threaded screws for fracture fixation in orthopedics: A finite element analysis[J]. Biomedical Physics & Engineering Express, 2021, 7(4):045010. [11] Jung B T, Kim W H, Park B, et al. Biomechanical evaluation of unilateral subcondylar fracture of the mandible on the varying materials: A finite element analysis[J]. PLoS One, 2020, 15(10):e0240352. [12] 冯佳男, 张文化, 雷洋. 闭合复位空心钉内固定与全髋关节置换术在移位型股骨颈骨折老年患者中的应用效果对比[J]. 临床和实验医学杂志, 2018, 17(13):1412-1415. [13] Staniger M P, Pietak A M, Huadmai J, et al. Magnesium and its alloys as orthopedic biomaterials: A review[J]. Biomaterials, 2006, 27(9):1728-1734. [14] Jia G Z, Hou Y, Chen C X, et al. Precise fabrication of open porous Mg scaffolds using NaCl templates: Relationship between space holder particles, pore characteristics and Mechanical behavior[J]. Materials & Design, 2018, 140:106-113. [15] Stroganov G B, Savitsky E, Mikhailovich, et al. Magnesium-base alloys for use in bone surgery: US Patent 3678135[P]. 1972. [16] 乔丽英, 高家诚, 王勇. 镁基生物材料表面改性及其生物相容性的研究与发展现状[J]. 中国材料进展, 2011, 30(4):23-29. [17] 张岩, 蒋垚. 镁基金属内植物腐蚀防护研究进展[J]. 国际骨科学杂志, 2008, 29(6):397-399. [18] Kuwahara H, Al-Abdullat Y, Mazaki N, et al. Precipitation of magnesium apatite on pure magnesium surface during immersing in Hank’s solution[J]. Materials Transactions, 2001, 42(7):1317-1321. [19] Mukherjee S, Barman S, Msndal N C, et al. Anti-bacterial activity of Achatina CRP and its mechanism of action[J]. Indian Journal of Experimental Biology, 2014, 52(7):692-704. [20] 王湛, 杨军, 李建军. 植入体内新型镁合金材料的抗菌性能[J]. 中国组织工程研究, 2018, 22(22):3451-3455. |
| 备注/Memo: | 收稿日期: 2021-10-27. 宁波大学学报(理工版)网址: http://journallg.nbu.edu.cn/ 基金项目: 河南省科技攻关重点项目(201402003). 第一作者: 方永刚(1979-), 男, 河南周口人, 副主任医师, 主要研究方向: 创伤骨科. E-mail: fyg19790730@163.com *通信作者: 张雁儒(1970-), 男, 河南西华人, 教授, 主要研究方向: 创伤骨科. E-mail: zyr@hpu.edu.cn 宁波大学学报(理工版)网址:http://journallg.nbu.edu.cn/ |